They are indeed lead-tin soldered. I suspect they were simply rust blued on a high polish and not allowed to etch during the rusting process. I've not tried this, but some of the advanced rust blueing techniques are used by some here.

I had a friend that had a BSS hot salt blued. It started coming apart within a year.