I do think Miller's idea of a 20g chamber sleeve is probably a safe solution as it adds wall to the chamber and reduces hoop stress from the smaller diameter at the same time. A sleeve from piece of 4140 or 4130, heat treated to about low 30s which would add tensile strength without overly reducing fatigue and fracture toughness, would be something to consider.