ChuckH is absolutely correct. HiForce solder flows at around 500 degrees Fahrenheit, considerably above the flow temp of the 60/40 lead/tin solder used on these old guns. There's really no need to use anything but 60/40 if all surfaces are scrupulously clean and properly fluxed.

Last edited by Ron Vella; 06/19/07 05:30 PM.